The ballast water system of an FPSO under construction was reassessed for pipe stress after the client commented on the assumptions in an earlier assessment. The system consists of two ballast pumps and twelve ballast tanks. Seawater is drawn from two sea inlet chests through two filters to the pump suctions, then discharged into a ring main that carries it to the tank being ballasted. The ring main and the suction and discharge lines to and from the pumps are Glass Reinforced Epoxy (GRE); the seawater intakes and the connecting piping to the tank nozzles are carbon steel.
The GRE pipe has a relatively low elasticity modulus, 10,000 MPa axial and 23,250 MPa hoop, which makes it grow under internal pressure in addition to its thermal expansion. The layout is relatively stiff, so the expansion from both pressure and temperature has to be accommodated by pipe bending.
Revised Inputs for the GRE Ballast System Reassessment
The earlier assessment had already identified stress problems. The client’s comments covered the minimum, normal and maximum operating temperatures and the applicable pressures, which led to additional load cases, and the assumed material properties.
In response to questions raised in the earlier assessment, the pipe supplier provided more detailed information. It confirmed that the flanges are rated for 16.0 barg (PN16) and the pipe is IPD-cured Bondstrand 7000M, and confirmed the internal diameters, wall thicknesses and all other assumed material properties. The shear modulus used previously was incorrect and was corrected to 6,400 MPa.
A site inspection checked the installed support configuration against the original support documentation. It found two deviations: an additional rest and guide support, and an altered support function in a branch of the pump P01 discharge. Both were included in the revised model.
CAESAR II Model, ISO 14692 Envelopes and Load Cases
The system was modelled in CAESAR II from the isometrics, the ballast system P&ID, pump data and pipe support detail drawings. Two approaches were available. Under API 15LR, every load case, including the static ones, would be checked against the cyclic long-term allowable stress envelope; this is conservative and would result in additional reinforcement requirements. ISO 14692-3 allows the static and cyclic loads to be separated, with each load type (occasional, operational or sustained) checked against its own non-factored long-term allowable stress envelope. The client agreed to the ISO 14692 approach.
The allowable stress envelope is a long-term envelope: the pipe material can sustain stresses within it for at least 20 years. It is derived from burst, axial tensile and long-term hydrostatic test data. For the static assessment of the installed pipe, the partial factors for temperature, chemical resistance and cyclic service are all 1.0. The resulting idealised long-term envelope has a factored stress of 140.6 MPa on the hoop axis and a long-term axial tensile strength of 24.1 MPa. A part factor f2 for each load type gives the non-factored envelopes: 0.89 for occasional loads such as the hydro test, 0.83 for the operational cases and 0.67 for the sustained cases.

Stress Envelope Results for the GRE Piping and Flanges
The system remained severely stressed. In the design case, 40 elements exceeded the static non-factored long-term allowable stress envelope on the axial tensile side, at a maximum of 152% of the allowable, and 39 elements exceeded it on the axial compressive side, at a maximum of 192%. In the maximum operating case, 25 elements exceeded the envelope on the tensile side, at a maximum of 134%, and 30 on the compressive side, at a maximum of 162%. In the other five load cases no element exceeded its envelope; the highest value, 92% of the allowable on the tensile side, was reached at two elements under the hydro test.
The design case is the most critical because thermal expansion has its largest effect there. The maximum operating case shows that excessive stresses can realistically occur during operation as well.
The exceedances mainly occur at fittings: bends and tees. The expansion is taken up by bending, and the stress intensification factors at these fittings make them the locations with the highest stresses. A top view of the model shows all elbows in the ring main and most of the tees outside the allowable envelope. Including the stiffness of the support steel structures is expected to raise the maximum combined axial stresses slightly, as it did in the earlier analysis.

Against the idealised short-term failure envelope, the highest combined axial stress was 37.1 MPa in the design case, 54% of the failure value. This appears to rule out immediate failure, but since the long-term allowable is exceeded, the risk of failure within a relatively short period will be large. The conclusion that no immediate failure will occur carries a reservation.
Short-term failure envelopes are generally based on a limited number of tests with potentially large scatter, and delaminations take time to develop, so short-term and long-term failure mechanisms often differ. The stress calculation assumes a linear stress-strain relation, which is no longer valid once stresses exceed the long-term envelope, and deviations between the installed and modelled support functions can influence the results. The calculations may therefore underestimate the real stress levels in excess of the long-term allowable.
The corrected shear modulus raised the maximum flange bending moment to 13,400 Nm at an ID 300 flange. This moment was assessed with the conservative equivalent pressure method, which converts the moment into an equivalent internal pressure, adds it to the real internal pressure and compares the sum with the flange allowable rating pressure (PN16). The moment exceeds the allowable at both the design pressure of 10.0 barg and the normal operating pressure of 4.0 barg. Only the moment from the maximum operating case, combined with the normal operating pressure, falls within it. Even that combination does not make the moment acceptable. The flange loads reach the absolute limits of the allowable levels, and reducing them is advised as part of the solution.
Flexibility Options for the Stiff GRE Ballast Layout
The cause of the exceedances is the lack of flexibility in the layout, which is a fundamental problem. Solving it by reinforcing the highly stressed areas alone is difficult. The first-order effect of reinforcement is further stiffening of the system and an increase in loads, which counteracts the mitigation. A solution has to come from increasing the layout flexibility.
The site inspection also checked two options for this. The first, raising the ring main with each ring-main tee rotated 90° to point vertically downward and each tank connection made through a 90° elbow to form a bending leg, was ruled out because other systems in the pump room make it impossible. The second inserts an expansion loop in each of the twelve ballast tank connections, with the ring main and pumps left at their current elevation and routing. The inspection showed this to be possible for at least eight of the twelve connections; the other four need further investigation.

Frequently Asked Questions
Why does GRE pipe grow under internal pressure?
The GRE pipe in this system has a relatively low elasticity modulus, 10,000 MPa axial and 23,250 MPa hoop. That makes it grow under internal pressure in addition to its thermal expansion. In a relatively stiff layout, the combined expansion from pressure and temperature has to be accommodated by pipe bending.
How does an ISO 14692-3 assessment of static loads differ from API 15LR?
API 15LR checks every load case, including the static ones, against the cyclic long-term allowable stress envelope. That is conservative and, for this system, would have resulted in additional reinforcement requirements. ISO 14692-3 allows static and cyclic loads to be separated, so each load type (occasional, operational or sustained) is checked against its own non-factored long-term allowable stress envelope.
Which part factors give the ISO 14692 non-factored envelope for each load type?
A part factor f2 is applied for each load type: 0.89 for occasional loads such as the hydro test, 0.83 for operational cases and 0.67 for sustained cases. In this assessment the static partial factors for temperature, chemical resistance and cyclic service were all 1.0. That gave an idealised long-term envelope with a factored stress of 140.6 MPa on the hoop axis and a long-term axial tensile strength of 24.1 MPa.
How far did the GRE ballast system exceed the ISO 14692 allowable envelope?
In the design case (50°C, 10.0 barg), 40 elements exceeded the static non-factored long-term allowable stress envelope on the axial tensile side, at a maximum of 152% of the allowable. On the compressive side, 39 elements exceeded it, at a maximum of 192%. The maximum operating case (45°C, 9.0 barg) still had 25 tensile and 30 compressive exceedances, at maxima of 134% and 162%. The other five load cases stayed within their envelopes.
Where do stress exceedances concentrate in a stiff GRE piping layout?
In this system they mainly occurred at fittings: bends and tees. With a stiff layout the expansion is taken up by bending, and the stress intensification factors at the fittings make them the most highly stressed locations. All elbows in the ring main and most of the tees were outside the allowable envelope.
Can reinforcement solve overstress in a stiff GRE layout?
Here the cause of the exceedances was the lack of flexibility in the layout. Solving that by reinforcing the highly stressed areas alone is difficult. The first-order effect of reinforcement is further stiffening of the system and an increase in loads, which counteracts the mitigation. A solution has to come from increasing the layout flexibility.
If GRE stresses are inside the short-term failure envelope, can immediate failure be ruled out?
Only with reservation. The highest combined axial stress was 37.1 MPa, 54% of the idealised short-term failure value, which appears to rule out immediate failure. Because the long-term allowable is exceeded, however, the risk of failure within a relatively short period will be large. There are three further limits on the short-term comparison:
- short-term failure envelopes are generally based on a limited number of tests with potentially large scatter;
- short-term and long-term failure mechanisms often differ, because delaminations take time to develop;
- a linear stress-strain calculation may underestimate stresses beyond the long-term envelope.
How were the GRE flange bending moments assessed?
With the conservative equivalent pressure method. The moment is converted into an equivalent internal pressure and added to the real internal pressure, and the sum is compared with the flange allowable rating pressure, here PN16. The maximum moment of 13,400 Nm at an ID 300 flange exceeded the allowable at both 10.0 barg and 4.0 barg, and reducing the flange bending loads is advised.
What options add flexibility to a stiff GRE ballast ring main?
Two were checked on site:
- Raising the ring main, with each tee rotated to point downward and each tank connection made through a 90° elbow forming a bending leg. This was ruled out by other systems in the pump room.
- An expansion loop in each ballast tank connection. This was found possible for at least eight of the twelve connections, with the other four needing further investigation.